Skip navigation
Please use this identifier to cite or link to this item: https://libeldoc.bsuir.by/handle/123456789/54123
Full metadata record
DC FieldValueLanguage
dc.contributor.authorGrevtsov, N.-
dc.contributor.authorChubenko, E.-
dc.contributor.authorBondarenko, V.-
dc.contributor.authorGavrilin, I.-
dc.contributor.authorDronov, A.-
dc.contributor.authorGavrilov, S.-
dc.contributor.authorRymski, G.-
dc.contributor.authorYanushkevich, K.-
dc.contributor.authorGoroshko, D.-
dc.contributor.authorArgunov, E.-
dc.coverage.spatialNetherlandsen_US
dc.date.accessioned2024-01-18T06:25:03Z-
dc.date.available2024-01-18T06:25:03Z-
dc.date.issued2023-
dc.identifier.citationComposition-Adjustable Silicon-Germanium Alloy Films based on Porous Silicon Matrices / N. Grevtsov [et al.] // Materials Today Communications. – 2023. – Vol. 38. – P. 107886.en_US
dc.identifier.urihttps://libeldoc.bsuir.by/handle/123456789/54123-
dc.description.abstractMorphology and crystalline structure of silicon-germanium alloys formed by rapid thermal processing of germanium-filled porous silicon layers are evaluated. Two types of porous silicon are employed as matrices for electrochemical pore filling using GeO2 aqueous solutions and subsequently compared, the first one formed by electrochemical anodization and the second by silver-assisted chemical etching of monocrystalline silicon. The resulting alloys’ structure and composition are investigated using scanning electron microscopy, energy-dispersive X-ray analysis, Raman spectroscopy and X-ray powder diffraction. It is shown that by varying the porosity of the initial matrix (by adjusting anodization current density for anodic porous silicon or changing silver deposition time for structures produced by metal-assisted etching) in the range from 55 to 75%, Si1-xGex alloys with germanium fractions of x = 0.31 to x = 0.83 can be formed, as indicated by Raman spectroscopy. It is concluded that composition-adjustable layers of silicon-germanium can be successfully formed on either type of porous silicon layer. While an increase in porosity generally leads to a decrease in silicon fractions in the alloy, the steepness of this effect varies heavily depending on the type of porous matrix used and should be considered independently for anodic porous silicon and silicon nanowires.en_US
dc.language.isoenen_US
dc.publisherElsevieren_US
dc.subjectпубликации ученыхen_US
dc.subjectnanomaterialsen_US
dc.subjectelectrochemical depositionen_US
dc.subjectchemical synthesisen_US
dc.subjectelectrodepositionen_US
dc.subjectsemiconductorsen_US
dc.subjectsilicon-germaniumen_US
dc.subjectthermoelectric materialsen_US
dc.subjectthin filmsen_US
dc.titleComposition-Adjustable Silicon-Germanium Alloy Films based on Porous Silicon Matricesen_US
dc.typeArticleen_US
dc.identifier.DOIDOI: 10.1016/j.mtcomm.2023.107886-
Appears in Collections:Публикации в зарубежных изданиях

Files in This Item:
File Description SizeFormat 
Composition_Grevtsov.pdf1.39 MBAdobe PDFView/Open
Show simple item record Google Scholar

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.