DC FieldValueLanguage
dc.contributor.authorTzaneva, B. R.-
dc.contributor.authorVrublevsky, I.-
dc.contributor.authorVidekov, V.-
dc.contributor.authorLushpa, N.-
dc.coverage.spatialGermanyen_US
dc.date.accessioned2025-01-23T11:27:01Z-
dc.date.available2025-01-23T11:27:01Z-
dc.date.issued2024-
dc.identifier.citationRole of electrode temperature in anodic growth of sulfuric acid alumina films / B. R. Tzaneva, I. Vrublevsky, V. Videkov, N. Lushpa // Journal of Solid State Electrochemistry. – 2024.en_US
dc.identifier.urihttps://libeldoc.bsuir.by/handle/123456789/58897-
dc.description.abstractStudies of the self-organized growth of nanoporous anodic aluminum oxide (AAO) films and anodization parameters have been the subject of decades of research and various theories. At the same time, temperature, being one of the most important parameters in anodizing treatments of aluminum, has been investigated only as a function of electrolyte temperature. This paper presents the results of studying the growth kinetics and morphology of AAO formed by anodization processes in 1 M H2SO4 at different anode temperatures. The activation energy of ionic conductivity for AAO determined in this study was 0.41 eV for sulfuric acid, which was greater than the activation energy of 0.34 eV for oxalic acid. The effect of anode temperature on the pore diameter (dpore) and the interpore distance (Dinter) was studied. It was demonstrated that in the temperature range from 10 to 40 °C, the dpore and Dinter did not change with the anode temperature, with values equal to 12.5 ± 0.1 nm and 52.5 ± 0.2 nm, respectively. However, when the anode (aluminum) temperature was increased to 60 °C, the dpore increased to 16 nm. The results obtained show that by increasing the temperature of the anode from 20 to 40 °C, it is possible to increase the ionic conductivity of AAO and thus achieve a greater than threefold increase in the the rate of AAO growth, without altering the porous morphology of the anodic films.en_US
dc.language.isoenen_US
dc.publisherSpringer Natureen_US
dc.subjectпубликации ученыхen_US
dc.subjectactivation energyen_US
dc.subjectanodic aluminaen_US
dc.subjectelectrode temperatureen_US
dc.subjectIonic conductivityen_US
dc.subjectsulfuric aciden_US
dc.titleRole of electrode temperature in anodic growth of sulfuric acid alumina filmsen_US
dc.typeArticleen_US
dc.identifier.DOIhttps://doi.org/10.1007/s10008-024-06036-9-
Appears in Collections:Публикации в зарубежных изданиях

Files in This Item:
File Description SizeFormat 
Role of electrode.pdf127.46 kBAdobe PDFView/Open
Show simple item record Google Scholar

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.