DC FieldValueLanguage
dc.contributor.authorStoliar, I. A.-
dc.contributor.authorShepelevich, V. G.-
dc.contributor.authorTashlykova-Bushkevich, I. I.-
dc.contributor.authorWu, R.-
dc.contributor.authorWendler, E.-
dc.coverage.spatialUSAen_US
dc.date.accessioned2026-01-06T09:58:47Z-
dc.date.available2026-01-06T09:58:47Z-
dc.date.issued2025-
dc.identifier.citationThe Influence of High-Temperature Heat Treatment on the Evolution of Surface Composition of Rapidly Solidified Foils of Al–Mg–Li–Sc–Zr Alloy / I. A. Stoliar, V. G. Shepelevich , I. I. Tashlykova [et al.] // Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques. – 2025. – Vol. 19. – No. 1. – P. 126–133.en_US
dc.identifier.urihttps://libeldoc.bsuir.by/handle/123456789/62622-
dc.description.abstractThe influence of high-temperature annealing on the composition of surface layers of rapidly solidified Al–Mg–Li–Sc–Zr alloy foils of 1421 grade obtained by centrifugal quenching from the melt has been studied when heated to 380°C in air depending on the holding time. Surface elemental mapping of the foils annealed for 1 h was carried out by scanning electron microscopy with energy dispersive X-ray microanalysis. The depth distribution of lithium after annealing the samples for 1, 2, and 8 h was studied by nuclear reaction analysis. After short-term annealing for 1 h, the formation of a gradient composition with an increased content of the main alloying elements in the surface layers of annealed foils was found. The thickness of the diffusion layer enriched with lithium is about 3.3 μm. In the 0.3-μm-thick near-surface layer, the average lithium concentration is 30 at %. In contrast to the contact surface, the nonmonotonic character of the lithium concentration profiles of the foils near the free surface includes the presence of a sharp maximum at a depth of 0.3 μm: the lithium content increases from 20 at % in the thin surface layer (0.1 μm) up to 40 at %. During the annealing process, with increasing holding time, an intensive mass transfer of lithium atoms to the depth of the foils is observed. The thickness of the diffusion layer increases 4 times.en_US
dc.language.isoenen_US
dc.publisherPleiades Publishingen_US
dc.subjectпубликации ученыхen_US
dc.subjectrapid solidification processingen_US
dc.subjectlithiumen_US
dc.subjectmagnesiumen_US
dc.subjectscanning electron microscopyen_US
dc.titleThe Influence of High-Temperature Heat Treatment on the Evolution of Surface Composition of Rapidly Solidified Foils of Al–Mg–Li–Sc–Zr Alloyen_US
dc.typeArticleen_US
Appears in Collections:Публикации в зарубежных изданиях

Files in This Item:
File Description SizeFormat 
Stoliar_The_Influence.pdf839.24 kBAdobe PDFView/Open
Show simple item record Google Scholar

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.