dc.date.issued2024-
dc.identifier.citationПоглотители электромагнитного излучения СВЧ-диапазона на основе никельсодержащего порошкообразного активированного древесного угля = Microwave absorbers based on nickel-containing powdered activated charcoal / О. В. Бойправ, В. А. Богуш, В. С. Мокеров, Е. С. Белоусова // Перспективные материалы. – 2024. – № 7. – С. 34–41.en_US
dc.identifier.urihttps://libeldoc.bsuir.by/handle/123456789/58887-
dc.description.abstractПредставлены и обоснованы закономерности изменения характеристик поглощения электромагнитного излучения в диапазоне частот 2,0 – 17,0 ГГц материалов на основе никельсодержащего порошкообразного активированного древесного угля в зависимости от технологии его получения. Материалы изготовлены путем заполнения частицами угля емкостей, сформированных из полимерной самоклеящейся пленки. Толщина материалов составляла 0,3 см, значения коэффициента поглощения электромагнитного излучения в диапазоне частот 2,0 – 17,0 ГГц достигают величины 0,9. Ширина эффективной полосы поглощения электромагнитного излучения материалов на основе никельсодержащего порошкообразного активированного древесного угля, полученного в процессе осаждения наночастиц в течение 5,0 мин, равна 10,0 ГГц, а при длительности осаждения 10,0 мин и 15,0 мин, — 10,6 ГГц и 10,8 ГГц соответственно. При этом среднее значение коэффициента поглощения электромагнитного излучения в эффективной полосе поглощения полученных материалов составило 0,75, 0,77 и 0,82 отн. ед. соответственно. Ширина эффективной полосы поглощения электромагнитного излучения материалов равна 6,7 ГГц, а их среднее значение коэффициента поглощения электромагнитного излучения в указанной полосе — 0,74 отн. ед. Полученные материалы могут быть использованы для обеспечения электромагнитной совместимости приборов электронной техники и СВЧ-устройств.en_US
dc.language.isoruen_US
dc.publisherООО «Интерконтакт Наука»en_US
dc.subjectпубликации ученыхen_US
dc.subjectкоэффициент поглощенияen_US
dc.subjectэлектромагнитное излучениеen_US
dc.subjectхимическое осаждениеen_US
dc.titleПоглотители электромагнитного излучения СВЧ-диапазона на основе никельсодержащего порошкообразного активированного древесного угляen_US
dc.title.alternativeMicrowave absorbers based on nickel-containing powdered activateden_US
dc.typeArticleen_US
dc.identifier.DOI10.30791/1028-978X-2024-7-34-41-
local.description.annotationThe patterns of changes in the electromagnetic radiation absorption characteristics in the frequency range 2.0 – 17.0 GHz of materials based on nickel-containing powdered activated charcoal are presented and substantiated depending on the duration of the process of nickel nanoparticles deposition from aqueous solutions implemented during its production. These materials are made by filling containers formed from a self-adhesive polymer film with particles of such coal. A foil-coated polymer film is attached to one of the outer surfaces of the walls of these containers. The thickness of these materials was 0.3 cm. It was established that their electromagnetic radiation absorption coefficient values in the frequency range 2.0 – 17.0 GHz reach of 0.9. The width of the electromagnetic radiation effective absorption band of materials based on nickel-containing powdered activated charcoal, during the production of which the duration of the process of nickel nanoparticles deposition was 5.0 min, is equal to 10.0 GHz, and for materials based on nickel-containing powdered activated charcoal, during the production in which the duration of the process of nickel nanoparticles deposition was 10.0 minutes and 15.0 minutes, 10.6 GHz and 10.8 GHz, respectively. The average value of electromagnetic radiation absorption coefficient in the effective absorption band of the listed materials is 0.75 rel. units, 0.77 rel. units and 0.82 rel. units respectively. It should be noted that the width of the electromagnetic radiation effective absorption band of materials manufactured in the above manner based on powdered activated charcoal is 6.7 GHz, and their average value of electromagnetic radiation absorption coefficient in the specified band is 0.74 rel. units The studied materials are among the basic materials of electronic technology and can be used to ensure electromagnetic compatibility of electronic devices, as well as microwave devices.en_US
Appears in Collections:Публикации в зарубежных изданиях

Files in This Item:
File Description SizeFormat 
Boiprav_Poglotiteli.pdf2.26 MBAdobe PDFView/Open
Show simple item record Google Scholar

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.